SA-688 TP 304LN Stainless Steels to SA-688/SA-688M

SA-688 TP 304LN - Specification & Application

  • SA-688/SA-688M - Specification for Welded Austenitic Stainless Steel Feedwater Heater Tubes

Specification for Welded Austenitic Stainless Steel Feedwater Heater Tubes

Chemical composition(wt.%) of SA-688 TP 304LN grade: to SA-688/SA-688M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.0 20.0
Ni 8.00 12.0
N 0.10 0.16

SA-688 TP 304LN - Detail

Specification for Welded Austenitic Stainless Steel Feedwater Heater Tubes

Mechanical properties of grade SA-688 TP 304LN SA-688/SA-688M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
566 (≥) 984 (≥) 23 11 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade SA-688 TP 304LN SA-688/SA-688M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
955 (≥) 776 (≥) 11 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
932 161 618