SA-693 S17700 Stainless Steels to SA-693

SA-693 S17700 - Specification & Application

  • SA-693 - Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of SA-693 S17700 grade: to SA-693

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.04
Cr 16.00 18.00
Ni 6.50 7.75
Mo - -
Al 0.75 1.50

SA-693 S17700 - Detail

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Mechanical properties of grade SA-693 S17700 SA-693

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
674 (≥) 675 (≥) 41 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade SA-693 S17700 SA-693

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
973 (≥) 951 (≥) 14 14 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
536 324 746
We can customize the production of SA-693 S17700 grade, contact us for the best solution.