SS 2360 Special Alloy

Chemical composition%of the ladle analysis of gradeSS 2360

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)
Max 0.12Max 1.0Max 2.0Max 0.045Max 0.03Min 19.0Min 18.0
Swedish SS standard stainless steel and heat resistant steel

Mechanical properties of gradeSS 2360

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
737(≥) 345(≥) 31 31 41 Solution and Aging,Annealing,Ausaging,Q+T,etc 333

Physical properties of grade SS 2360

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
459(≥) 953(≥) 22 12 33 Solution and Aging,Annealing,Ausaging,Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
988 889 139

SS 2360 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED