SS 2377 Special Alloy

Chemical composition%of the ladle analysis of gradeSS 2377

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)N(%)
Max 0.030Max 1.0Max 2.0Max 0.03Max 0.0221.0-23.04.5-6.52.5-3.50.10-0.20
Swedish SS standard stainless steel and heat resistant steel

Mechanical properties of gradeSS 2377

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
484(≥) 961(≥) 33 14 32 Solution and Aging,Annealing,Ausaging,Q+T,etc 224

Physical properties of grade SS 2377

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
124(≥) 491(≥) 14 31 23 Solution and Aging,Annealing,Ausaging,Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
261 213 617

SS 2377 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED