STS310STP Stainless Steels to D 3576 (2011)

STS310STP - Specification & Application

  • D 3576 (2011) - Stainless steel pipes
  • D 9536 (2011) - Stainless lined steel pipe

Stainless lined steel pipe

Chemical composition(wt.%) of STS310STP grade: to D 3576 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.030
Cr 24.00 26.00
Ni 19.00 22.00
Mo - -
N - -

STS310STP - Detail

Stainless lined steel pipe

Mechanical properties of grade STS310STP D 3576 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
768 (≥) 822 (≥) 41 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade STS310STP D 3576 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
335 (≥) 487 (≥) 32 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
934 361 557

Equivalent Products

We can customize the production of STS310STP grade, contact us for the best solution.