STS316TPD Stainless Steels to D 3595 (2010)

STS316TPD - Specification & Application

  • D 3595 (2010) - Light gauge stainless steel pipes for ordinary piping
  • D 9536 (2011) - Stainless lined steel pipe

Stainless lined steel pipe

Chemical composition(wt.%) of STS316TPD grade: to D 3595 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.00 18.00
Ni 10.00 14.00
Mo 2.00 3.00
N - -

STS316TPD - Detail

Stainless lined steel pipe

Mechanical properties of grade STS316TPD D 3595 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
679 (≥) 442 (≥) 42 31 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade STS316TPD D 3595 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
926 (≥) 113 (≥) 42 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
659 147 352

Equivalent Products

We can customize the production of STS316TPD grade, contact us for the best solution.