STS317 Stainless Steels to D 3698 (2008)

STS317 - Specification & Application

  • D 3698 (2008) - Cold rolled stainless steel plates, sheets and strip
  • D 3702 (2008) - Stainless steel wire rods
  • D 3703 (2007) - Stainless steel wires
  • D 3705 (2008) - Hot rolled stainless steel plates, sheets and strip
  • D 3706 (2008) - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of STS317 grade: to D 3698 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 18.00 20.00
Ni 11.00 15.00
Mo 3.00 4.00
N - -

STS317 - Detail

Stainless steel bars

Mechanical properties of grade STS317 D 3698 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
467 (≥) 738 (≥) 14 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade STS317 D 3698 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
425 (≥) 397 (≥) 12 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
716 613 676

Equivalent Products

We can customize the production of STS317 grade, contact us for the best solution.