STS410J1 Stainless Steels to D 3706 (2008)

STS410J1 - Specification & Application

  • D 3706 (2008) - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of STS410J1 grade: to D 3706 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.18
Si - 0.60
Mn - 1.00
P - 0.040
S - 0.030
Cr 11.50 14.00
Ni - 0.60
Mo 0.30 0.60
N - -

STS410J1 - Detail

Stainless steel bars

Mechanical properties of grade STS410J1 D 3706 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
853 (≥) 597 (≥) 32 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade STS410J1 D 3706 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
211 (≥) 932 (≥) 34 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
956 232 679

Equivalent Grade

Equivalent Products

We can customize the production of STS410J1 grade, contact us for the best solution.