STS430LXTB Stainless Steels to D 3577 (2007)

STS430LXTB - Specification & Application

  • D 3577 (2007) - Stainless steel for boiler and heat exchanger tubes

Stainless steel for boiler and heat exchanger tubes

Chemical composition(wt.%) of STS430LXTB grade: to D 3577 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 1.00
P - 0.040
S - 0.030
Cr 16.00 19.00
Ni - 0.60
Mo - -
N - -
Ti/Nb 0.10 1.00

STS430LXTB - Detail

Stainless steel for boiler and heat exchanger tubes

Mechanical properties of grade STS430LXTB D 3577 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
479 (≥) 212 (≥) 32 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade STS430LXTB D 3577 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
659 (≥) 857 (≥) 12 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
374 697 644

Equivalent Products

We can customize the production of STS430LXTB grade, contact us for the best solution.