SUH 11M Stainless Steels to SAE J 775 (2004)

SUH 11M - Specification & Application

  • SAE J 775 (2004) - Engine poppet valve information report

Engine poppet valve information report

Chemical composition(wt.%) of SUH 11M grade: to SAE J 775 (2004)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.47 0.55
Si 1.00 2.00
Mn - 0.60
Cr 7.50 9.50
Ni - 0.60
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - -
P - 0.03
S - 0.03

SUH 11M - Detail

Engine poppet valve information report

Mechanical properties of grade SUH 11M SAE J 775 (2004)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
675 (≥) 162 (≥) 22 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade SUH 11M SAE J 775 (2004)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
896 (≥) 299 (≥) 23 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
231 452 333

Equivalent Grade

Equivalent Products