SUS304L Stainless Steels to SA/JIS G4303

SUS304L - Specification & Application

  • SA/JIS G4303 - Specification for stainless steel bars

Specification for stainless steel bars

Chemical composition(wt.%) of SUS304L grade: to SA/JIS G4303

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 9.00 13.00

SUS304L - Detail

Specification for stainless steel bars

Mechanical properties of grade SUS304L SA/JIS G4303

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
182 (≥) 773 (≥) 12 43 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade SUS304L SA/JIS G4303

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
459 (≥) 867 (≥) 34 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
823 387 498
We can customize the production of SUS304L grade, contact us for the best solution.