Stellite 159 Tool Die Steels

Stellite 159 - Specification & Application

Stellite alloy

Chemical composition(wt.%) of Stellite 159 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 3.30
Mn - -
Cr - 18.50
Ni - 27.00
Mo - 5.50
Co remaining -
W - -
Fe - 2.00
B - 3.20

Stellite 159 - Detail

Stellite alloy

Mechanical properties of grade Stellite 159

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
211 (≥) 311 (≥) 33 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade Stellite 159

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
593 (≥) 144 (≥) 22 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
177 297 477

Equivalent Grade

Equivalent Products

We can customize the production of Stellite 159 grade, contact us for the best solution.