Stellite 694 Tool Die Steels

Stellite 694 - Specification & Application

Stellite alloy

Chemical composition(wt.%) of Stellite 694 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.85
Si - 1.00
Mn - 1.00
Cr - 28.00
Ni - 5.00
Mo - -
Co remaining -
W - 19.50
Fe - 3.00
V - 1.00
B - 0.010

Stellite 694 - Detail

Stellite alloy

Mechanical properties of grade Stellite 694

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
188 (≥) 447 (≥) 14 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade Stellite 694

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
332 (≥) 135 (≥) 31 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
496 389 744

Equivalent Grade

Equivalent Products

We can customize the production of Stellite 694 grade, contact us for the best solution.
sales@specificsteel.com