T12006 Tool Die Steels

T12006 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of T12006 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.75 0.85
Si 0.20 0.40
Mn 0.20 0.40
P - 0.030
S - 0.030
Cr 4.00 4.75
Mo 0.40 1.00
V 1.50 2.10
W 18.50 21.00
Co 11.00 13.00

T12006 - Detail

High-Speed Tool Steel

Mechanical properties of grade T12006

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
334 (≥) 931 (≥) 33 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade T12006

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
643 (≥) 735 (≥) 43 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
323 118 285

Equivalent Grade

Equivalent Products

We can customize the production of T12006 grade, contact us for the best solution.