Hot-Work Tool Steel

Chemical composition(wt.%) of T20814 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 0.80 1.20
Mn 0.20 0.50
P - 0.030
S - 0.030
Cr 4.75 5.50
Mo - -
V - -
W 4.00 5.25
Ni+Cu - 0.75

T20814 - Detail

Hot-Work Tool Steel

Mechanical properties of grade T20814

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
451 (≥) 961 (≥) 24 43 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade T20814

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
913 (≥) 123 (≥) 22 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
518 695 143