T31506 Tool Die Steels

T31506 - Specification & Application

Oil-Hardening Tool Steel

Chemical composition(wt.%) of T31506 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.25 1.55
Si 0.55 1.50
Mn 0.30 1.10
P - 0.030
S - 0.030
Cr - 0.30
Mo 0.20 0.30
V - -
W - -
Ni+Cu - 0.75

T31506 - Detail

Oil-Hardening Tool Steel

Mechanical properties of grade T31506

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
725 (≥) 752 (≥) 44 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade T31506

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
761 (≥) 852 (≥) 13 41 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 224
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
899 293 966

Equivalent Grade

Equivalent Products

We can customize the production of T31506 grade, contact us for the best solution.