T31507 Tool Die Steels

T31507 - Specification & Application

Oil-Hardening Tool Steel

Chemical composition(wt.%) of T31507 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.10 1.30
Si 0.10 0.60
Mn 0.20 1.00
P - 0.030
S - 0.030
Cr 0.35 0.85
Mo - 0.30
V 0.15 0.40
W 1.00 2.00
Ni+Cu - 0.75

T31507 - Detail

Oil-Hardening Tool Steel

Mechanical properties of grade T31507

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
325 (≥) 119 (≥) 42 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade T31507

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
784 (≥) 573 (≥) 24 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
846 876 387

Equivalent Grade

Equivalent Products

We can customize the production of T31507 grade, contact us for the best solution.