T5 Tool Die Steels

T5 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of T5 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.75 0.85
Si 0.20 0.40
Mn 0.20 0.40
P - 0.030
S - 0.030
Cr 3.75 5.00
Mo 0.50 1.25
V 1.80 2.40
W 17.50 19.00
Co 7.00 9.50

T5 - Detail

High-Speed Tool Steel

Mechanical properties of grade T5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
835 (≥) 313 (≥) 11 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade T5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
288 (≥) 263 (≥) 21 41 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
743 583 737
We can customize the production of T5 grade, contact us for the best solution.