Udimet 500 Stainless Steels to SAE AMS 5751E (1982)

Udimet 500 - Specification & Application

  • SAE AMS 5751E (1982) - Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant 54Ni - 17.5Cr - 16.5Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Solution, Stabilization, and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted

Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant 54Ni - 17.5Cr - 16.5Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Solution, Stabilization, and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted

Chemical composition(wt.%) of Udimet 500 grade: to SAE AMS 5751E (1982)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Si - 0.10
Mn - 0.10
Cr - 19.00
Ni - remaining
Mo - 4.00
Co - 19.00
W - -
Al - 3.00
Cu - -
Ti - 3.00
Fe - -
Zr - 0.06
B - 0.005

Udimet 500 - Detail

Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant 54Ni - 17.5Cr - 16.5Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Solution, Stabilization, and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted

Mechanical properties of grade Udimet 500 SAE AMS 5751E (1982)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
995 (≥) 814 (≥) 32 24 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade Udimet 500 SAE AMS 5751E (1982)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
315 (≥) 364 (≥) 31 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
159 335 841

Equivalent Products

We can customize the production of Udimet 500 grade, contact us for the best solution.