W Special Alloy

Chemical composition%of the ladle analysis of gradeW

C(%)Si(%)Mn(%)Cr(%)W(%)
1.05~1.25≤0.40≤0.400.10~0.300.80~1.20
  • » Alloy steel the performance characteristic and the USES(4)
  • » Alloy steel the performance characteristic and the USES(3)
  • » Alloy steel the performance characteristic and the USES(2)
  • » Alloy steel the performance characteristic and the USES(1)
  • Mechanical properties of gradeW

    Proof strength
    Rp0.2(MPa)
    Tensile strength
    Rm(MPa)
    Impact energy
    KV(J)
    Elongation at fracture
    A(%)
    Reduction in cross section on fracture
    Z(%)
    As-Heat-Treated Condition Brinell hardness(HBW)
    445(≥) 276(≥) 41 34 14 Solution and Aging,Annealing,Ausaging,Q+T,etc 122

    Physical properties of grade W

    Property Density
    kg/dm3
    Temperature T
    °C/F
    Specific heat
    J/kgK
    Thermal conductivity
    W/mK
    Electric resistance
    µΩ·cm
    Modulus of elasticity
    kN/mm2
    Expansion rate
    852(≥) 668(≥) 11 14 21 Solution and Aging,Annealing,Ausaging,Q+T,etc 212
    Temp.
    °C/°F
    Creep strain limit
    (10000h)
    (Rp1,0)N/mm2
    Creep rupture strength
    (10000h)
    (Rp1,0)N/mm2
    353 475 265

    W Range of products

    Product type Products Dimension Processes Deliver Status
    Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
    Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
    Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
    Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

    W Steel Stock

    Steel grade Dimension Shape Unit Quantity Delivery state Query
    Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
    1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
    1Cr11Ni2W2MoV,961,13Cr11Ni2W2MoV Sheet Select 0 Select Enquiry