X160CrMoV12 / Z160CDV12 Tool Die Steels to NF A35-590(1992)

X160CrMoV12 / Z160CDV12 - Specification & Application

  • NF A35-590(1992) -

Cold working alloy tool steels

Chemical composition(wt.%) of X160CrMoV12 / Z160CDV12 grade: to NF A35-590(1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.45 1.70
Si 0.10 0.40
Mn 0.15 0.45
Cr 11.0 13.0
Mo 0.70 1.10
V 0.70 1.00

X160CrMoV12 / Z160CDV12 - Detail

X160CrMoV12

Mechanical properties of grade X160CrMoV12 / Z160CDV12 NF A35-590(1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
138 (≥) 882 (≥) 21 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade X160CrMoV12 / Z160CDV12 NF A35-590(1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
866 (≥) 417 (≥) 41 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
623 346 591
We can customize the production of X160CrMoV12 / Z160CDV12 grade, contact us for the best solution.
sales@specificsteel.com