X36CrMo17 Tool Die Steels to DIN 17350 (1980)

X36CrMo17 - Specification & Application

  • DIN 17350 (1980) - Tool Steels; Technical Conditions of Delivery

Tool Steels; Technical Conditions of Delivery

Chemical composition(wt.%) of X36CrMo17 grade: to DIN 17350 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.33 0.43
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.030
Cr 15.00 17.00
Mo 1.00 1.30
V - -
Ni - 1.00

X36CrMo17 - Detail

Tool Steels; Technical Conditions of Delivery

Mechanical properties of grade X36CrMo17 DIN 17350 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
719 (≥) 268 (≥) 13 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade X36CrMo17 DIN 17350 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
767 (≥) 529 (≥) 12 42 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
848 478 729

Equivalent Grade

Equivalent Products