X5CrNiN18-8 Stainless Steels to ISO/TS 15510 (2003)

X5CrNiN18-8 - Specification & Application

  • ISO/TS 15510 (2003) - Stainless steels - Chemical composition

Stainless steels - Chemical composition

Chemical composition(wt.%) of X5CrNiN18-8 grade: to ISO/TS 15510 (2003)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 1.00
Mn - 2.50
P - 0.045
S - 0.030
Cr 17.00 19.50
Ni 7.00 10.50
Mo - -
N 0.10 0.16

X5CrNiN18-8 - Detail

Stainless steels - Chemical composition

Mechanical properties of grade X5CrNiN18-8 ISO/TS 15510 (2003)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
133 (≥) 369 (≥) 44 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade X5CrNiN18-8 ISO/TS 15510 (2003)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
417 (≥) 772 (≥) 43 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
156 121 781

Equivalent Grade

Equivalent Products

We can customize the production of X5CrNiN18-8 grade, contact us for the best solution.