XH33TMДЮ(ЭK63,BHC-45) Stainless Steels

XH33TMДЮ(ЭK63,BHC-45) - Specification & Application

Russia TY standard corrosion resistant alloy hot rolled and forged bars

Chemical composition(wt.%) of XH33TMДЮ(ЭK63,BHC-45) grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.01 0.05
Si - 0.40
Mn 1.00 1.50
S 0.15 0.25
P 0.06 0.12
Cr 13.00 15.00
Ni 32.00 35.00
Mo 1.50 2.00
Ti 2.50 3.00
Al 0.70 1.00
Cu 1.00 1.50
Ca - 0.05

XH33TMДЮ(ЭK63,BHC-45) - Detail

Russia TY standard corrosion resistant alloy hot rolled and forged bars

Mechanical properties of grade XH33TMДЮ(ЭK63,BHC-45)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
925 (≥) 785 (≥) 42 23 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade XH33TMДЮ(ЭK63,BHC-45)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
127 (≥) 117 (≥) 11 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
147 561 695

Equivalent Grade

Equivalent Products

We can customize the production of XH33TMДЮ(ЭK63,BHC-45) grade, contact us for the best solution.
sales@specificsteel.com