XM15J1 Stainless Steels to G3067

XM15J1 - Specification & Application

  • G3067 - Stainless steel bars
  • G3076 - Stainless steel wires

Stainless steel wires

Chemical composition(wt.%) of XM15J1 grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si 3.00 5.00
Mn - 2.00
P - 0.045
S - 0.030
Ni 11.50 15.00
Cr 15.00 20.00
Mo - -

XM15J1 - Detail

Stainless steel wires

Mechanical properties of grade XM15J1 G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
431 (≥) 844 (≥) 13 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade XM15J1 G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
762 (≥) 594 (≥) 41 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
396 265 563

Equivalent Products

We can customize the production of XM15J1 grade, contact us for the best solution.