Z15CNS25-20 Stainless Steels to NF A 35-590

Z15CNS25-20 - Specification & Application

  • NF A 35-590 - Tool steels
  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips
  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application
  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Chemical composition(wt.%) of Z15CNS25-20 grade: to NF A 35-590

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 1.50 2.50
Mn - 2.00
P - 0.040
S - 0.015
Cr 24.00 26.00
Mo - -
Ni 19.00 21.00

Z15CNS25-20 - Detail

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Mechanical properties of grade Z15CNS25-20 NF A 35-590

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
777 (≥) 454 (≥) 13 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade Z15CNS25-20 NF A 35-590

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
861 (≥) 629 (≥) 31 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
785 549 737

Equivalent Grade

Equivalent Products

We can customize the production of Z15CNS25-20 grade, contact us for the best solution.