Z6CNDT17-12 Stainless Steels to NF A 36-607

Z6CNDT17-12 - Specification & Application

  • NF A 36-607 - Austenitic stainless steel parts obtained by flat die forging or drop forging for boilers and pressure vessels. Grade and types
  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips
  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod
  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application
  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Chemical composition(wt.%) of Z6CNDT17-12 grade: to NF A 36-607

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.060
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 16.00 18.00
Mo 2.00 2.50
Ni 10.50 12.50
N - 0.020
Ti 5(C+N) 0.70

Z6CNDT17-12 - Detail

Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels

Mechanical properties of grade Z6CNDT17-12 NF A 36-607

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
489 (≥) 949 (≥) 11 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade Z6CNDT17-12 NF A 36-607

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
661 (≥) 633 (≥) 13 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
769 628 853

Equivalent Products

We can customize the production of Z6CNDT17-12 grade, contact us for the best solution.