Z7CNU16-04 Stainless Steels to NF A 35-574

Z7CNU16-04 - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(wt.%) of Z7CNU16-04 grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.070
Si - 0.75
Mn - 1.00
P - 0.035
S - 0.025
Cr 15.00 17.50
Mo - 0.50
Ni 3.00 5.00
Cu 3.00 5.00
Nb+Ta 0.15 0.45

Z7CNU16-04 - Detail

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Mechanical properties of grade Z7CNU16-04 NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
466 (≥) 364 (≥) 12 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade Z7CNU16-04 NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
927 (≥) 124 (≥) 22 32 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
213 115 337

Equivalent Grade

Equivalent Products

We can customize the production of Z7CNU16-04 grade, contact us for the best solution.
sales@specificsteel.com