X100CrMoV5-1 Tool Die Steels

X100CrMoV5-1 - Specification & Application

Alloyed CrMoV steel

Chemical composition(wt.%) of X100CrMoV5-1 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.90 1.05
Si 0.20 0.40
Mn 0.40 0.70
P - 0.035
S - 0.035
Cr 4.80 5.50
Mo 0.90 1.20
V 0.10 0.30

X100CrMoV5-1 - Detail

Alloyed CrMoV steel

Mechanical properties of grade X100CrMoV5-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
532 (≥) 877 (≥) 11 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade X100CrMoV5-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
826 (≥) 458 (≥) 43 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
617 984 821

Equivalent Grade

Equivalent Products

We can customize the production of X100CrMoV5-1 grade, contact us for the best solution.
sales@specificsteel.com