X3CrNiMoN27-5-2 Stainless Steels to BS EN 10088-1

X3CrNiMoN27-5-2 - Specification & Application

  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • BS EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • BS EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
  • BS EN 10297-2 (2005) - Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Chemical composition(wt.%) of X3CrNiMoN27-5-2 grade: to BS EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.015
Cr 25.00 28.00
Ni 4.50 6.50
Mo 1.30 2.00
N 0.50 0.20

X3CrNiMoN27-5-2 - Detail

Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel

Mechanical properties of grade X3CrNiMoN27-5-2 BS EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
513 (≥) 287 (≥) 21 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade X3CrNiMoN27-5-2 BS EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
745 (≥) 656 (≥) 43 11 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
479 623 477

Equivalent Products

We can customize the production of X3CrNiMoN27-5-2 grade, contact us for the best solution.
sales@specificsteel.com