ЖC3-BИ Stainless Steels

ЖC3-BИ - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of ЖC3-BИ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.11 0.16
Cr 14.00 18.00
Ni - remaining
Co - -
Mo 3.00 4.50
W 4.50 6.50
Al 1.60 2.20
Ti 1.60 2.30
Nb - -
Fe - 8.00

ЖC3-BИ - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade ЖC3-BИ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
425 (≥) 685 (≥) 42 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade ЖC3-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
446 (≥) 244 (≥) 22 34 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
913 173 788

Equivalent Products

We can customize the production of ЖC3-BИ grade, contact us for the best solution.
sales@specificsteel.com