Russia GOCT Standard vacuum smelting casting high temperature alloy bar
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
Si | - | 0.60 | ||
Mn | - | 0.60 | ||
P | - | 0.015 | ||
S | - | 0.009 | ||
B | 0.005 | 0.010 | ||
Ce | - | - | ||
Zr | - | - | ||
Y | - | - | ||
Pb | - | - | ||
Bi | - | - | ||
V | - | 0.30 |
Russia GOCT Standard vacuum smelting casting high temperature alloy bar
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
169 (≥) | 889 (≥) | 13 | 33 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
825 (≥) | 691 (≥) | 34 | 41 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 214 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
914 | 123 | 527 |
We can customize the production of ЖC3-BИ grade, contact us for the best solution.