00Cr17Mo Stainless Steels to GB/T 3280 (1992)

00Cr17Mo - Specification & Application

  • GB/T 3280 (1992) - Cold rolled stainless steel sheets and plates
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • GB/T 4239 (1991) - Cold rolled stainless steel and heat resisting steel strips

Cold rolled stainless steel sheets and plates

Chemical composition(wt.%) of 00Cr17Mo grade: to GB/T 3280 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 1.00
Mn - 1.00
P - 0.035
S - 0.030
Ni - 0.60
Cr 16.00 19.00
Mo 0.75 1.25
Ti+Nb+Zr - 8x(C%+N%)-0.80
N - 0.025

00Cr17Mo - Detail

00Cr17Mo

Mechanical properties of grade 00Cr17Mo GB/T 3280 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
825 (≥) 325 (≥) 13 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade 00Cr17Mo GB/T 3280 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
627 (≥) 463 (≥) 42 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
792 685 863

Equivalent Grade

Equivalent Products

We can customize the production of 00Cr17Mo grade, contact us for the best solution.