00Cr18Ni5Mo3Si2 Stainless Steels to GB/T 1220 (1992)

00Cr18Ni5Mo3Si2 - Specification & Application

  • GB/T 1220 (1992) - Stainless steel bars
  • GB/T 14975 (2002) - Stainless steel seamless tubes for structures
  • GB/T 14976 (2002) - Stainless steel seamless tubes for fluid transport
  • GB/T 3280 (2007) - Cold rolled stainless steel sheets and plates
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • JB 4728 (2000) - Stainless steel forgings for pressure vessels

Stainless steel bars

Chemical composition(wt.%) of 00Cr18Ni5Mo3Si2 grade: to GB/T 1220 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si 1.30 2.00
Mn 1.00 2.00
P - 0.035
S - 0.030
Ni 4.50 5.50
Cr 18.00 19.50
Mo 2.50 3.00

00Cr18Ni5Mo3Si2 - Detail

00Cr18Ni5Mo3Si2 Stainless steel bars

Mechanical properties of grade 00Cr18Ni5Mo3Si2 GB/T 1220 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
336 (≥) 131 (≥) 24 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade 00Cr18Ni5Mo3Si2 GB/T 1220 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
158 (≥) 773 (≥) 41 41 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
847 516 746

Equivalent Products

We can customize the production of 00Cr18Ni5Mo3Si2 grade, contact us for the best solution.