03X17H14M2 Stainless Steels

03X17H14M2 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 03X17H14M2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.40
Mn 1.00 2.00
P - 0.035
S - 0.020
Cr 16.00 18.00
Ni 13.00 15.00
Mo 2.50 3.10
W - 0.20
Ti - 0.20

03X17H14M2 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 03X17H14M2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
286 (≥) 576 (≥) 24 44 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade 03X17H14M2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
596 (≥) 838 (≥) 12 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
748 812 694

Equivalent Grade

Equivalent Products

We can customize the production of 03X17H14M2 grade, contact us for the best solution.