0Cr17Ni12Mo2 Stainless Steels to GB 13296 (2007)

0Cr17Ni12Mo2 - Specification & Application

  • GB 13296 (2007) - Seamless stainless steel tubes for boiler and heat exchanger
  • GB 4238 (1992) - Heat-resisting steel sheets and plates
  • GB/T 1220 (1992) - Stainless steel bars
  • GB/T 1221 (1992) - Heat-resisting steel bars
  • GB/T 12770 (2002) - Welded stainless steel tubes for machine structures
  • GB/T 12771 (2000) - Welded stainless steel pipes for liquid delivery
  • GB/T 14975 (2002) - Stainless steel seamless tubes for structures
  • GB/T 14976 (2002) - Stainless steel seamless tubes for fluid transport
  • GB/T 3090 (2000) - Stainless steel small diameter seamless steel tubes
  • GB/T 3280 (2007) - Cold rolled stainless steel sheets and plates
  • GB/T 4226 (2004) - Cold finished stainless steel bars
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • GB/T 4239 (1991) - Cold rolled stainless steel and heat resisting steel strips
  • GB/T 4240 (1993) - Stainless steel wires
  • GB/T 4356 (2002) - Stainless steel wire rods
  • JB 4728 (2000) - Stainless Steel Forgings for Pressure Vessels

Seamless stainless steel tubes for boiler and heat exchanger

Chemical composition(wt.%) of 0Cr17Ni12Mo2 grade: to GB 13296 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.030
Ni 10.00 14.00
Cr 16.00 18.50
Mo 2.00 3.00

0Cr17Ni12Mo2 - Detail

0Cr17Ni12Mo2

Mechanical properties of grade 0Cr17Ni12Mo2 GB 13296 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
477 (≥) 915 (≥) 22 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade 0Cr17Ni12Mo2 GB 13296 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
376 (≥) 341 (≥) 24 42 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
818 647 195

Equivalent Products

We can customize the production of 0Cr17Ni12Mo2 grade, contact us for the best solution.
sales@specificsteel.com