0Cr18Ni12Mo2Cu2 stainless steel corrosion resistance, resistance to corrosion resistance is better than 0Cr17Ni12Mo2. 0Cr18Ni12Mo2Cu2 stainless steel used in the sulphuric acid resistant material.

Chemical composition(wt.%) of 0Cr18Ni12Mo2Cu2 grade: to GB/T 1220-1992

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.030
Ni 10.00 14.50
Cr 17.00 19.00
Mo 1.20 2.75
Cu 1.00 2.50

0Cr18Ni12Mo2Cu2 - Detail

0Cr18Ni12Mo2Cu2

Mechanical properties of grade 0Cr18Ni12Mo2Cu2 GB/T 1220-1992

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
267 (≥) 832 (≥) 14 21 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade 0Cr18Ni12Mo2Cu2 GB/T 1220-1992

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
676 (≥) 649 (≥) 24 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
569 133 576

Equivalent Grade

Equivalent Products

We can customize the production of 0Cr18Ni12Mo2Cu2 grade, contact us for the best solution.