0Cr19Ni10NbN Stainless Steels to GB/T 1220 (1992)

0Cr19Ni10NbN - Specification & Application

  • GB/T 1220 (1992) - Austenitic stainless steel bars
  • GB/T 14976 (2002) - Stainless steel seamless tubes for fluid transport
  • GB/T 3280 (2007) - Cold rolled stainless steel sheets and plates
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • GB/T 4239 (1991) - Cold rolled stainless steel and heat resisting steel strips

Based on zero cr19ni9 plus N and Nb, with better than 0 cr19ni9 properties and USES

Chemical composition(wt.%) of 0Cr19Ni10NbN grade: to GB/T 1220 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.030
Ni 7.50 10.50
Cr 18.00 20.00
Nb - 0.15
N 0.15 0.30

0Cr19Ni10NbN - Detail

Stainless and heat resisting steels
Austenitic stainless steel bars

Mechanical properties of grade 0Cr19Ni10NbN GB/T 1220 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
653 (≥) 995 (≥) 24 44 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade 0Cr19Ni10NbN GB/T 1220 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
525 (≥) 521 (≥) 34 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
423 426 993

Equivalent Grade

Equivalent Products

We can customize the production of 0Cr19Ni10NbN grade, contact us for the best solution.