1.4594 Stainless Steels to BS EN 10088-1

1.4594 - Specification & Application

  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Chemical composition(wt.%) of 1.4594 grade: to BS EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 0.70
Mn - 1.00
P - 0.04
S - 0.015
Cr 13.00 15.00
Ni 5.00 6.00
Mo 1.20 2.00
Nb+Ta 0.15 0.60
Cu 1.20 2.00

1.4594 - Detail

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Mechanical properties of grade 1.4594 BS EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
354 (≥) 862 (≥) 41 22 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade 1.4594 BS EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
631 (≥) 395 (≥) 11 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
893 628 346

Equivalent Products

We can customize the production of 1.4594 grade, contact us for the best solution.