1.4872 Stainless Steels to BS EN 10088-1

1.4872 - Specification & Application

  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10095 - Heat resisting steels and nickel alloys

Heat resisting steels and nickel alloys

Chemical composition(wt.%) of 1.4872 grade: to BS EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.30
Si - 1.00
Mn 8.00 10.00
P - 0.045
S - 0.015
Cr 24.00 26.00
Ni 6.00 8.00
Al - -
N 0.20 0.40

1.4872 - Detail

Heat resisting steels and nickel alloys

Mechanical properties of grade 1.4872 BS EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
232 (≥) 189 (≥) 44 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade 1.4872 BS EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
342 (≥) 765 (≥) 12 42 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
454 959 297

Equivalent Products

We can customize the production of 1.4872 grade, contact us for the best solution.