Flat products made of steels for pressure purposes. Non-alloy and alloy steels with specified elevated temperature properties
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.17 | ||
Si | 0.50 | 0.80 | ||
Mn | 0.40 | 0.65 | ||
P | - | 0.015 | ||
S | - | 0.005 | ||
Cr | 1.00 | 1.50 | ||
Ni | - | 0.30 | ||
Mo | 0.45 | 0.65 | ||
N | - | 0.012 | ||
Cu | - | 0.013 |
EN 1.7336 steel is an alloy steel formulated for primary forming into wrought products. 1.7336 is the EN numeric designation for this material. 13CrMoSi5-5 is the EN chemical designation. It has a moderately low thermal conductivity among EN wrought alloy steels. In addition, it has a moderately high base cost and a fairly low tensile strength.
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
674 (≥) | 724 (≥) | 21 | 24 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 444 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
277 (≥) | 826 (≥) | 13 | 21 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
182 | 791 | 213 |
We can customize the production of 1.7336 grade, contact us for the best solution.