17-4PH Special Alloy

Chemical composition%of the ladle analysis of grade17-4PH

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Cu(%)Nb(%)
0.0711Max 0.04Max 0.0315.5-17.53.00-5.003.00-5.000.15-0.45
17-4PH

Mechanical properties of grade17-4PH

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
281(≥) 641(≥) 14 43 13 Solution and Aging,Annealing,Ausaging,Q+T,etc 342

Physical properties of grade 17-4PH

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
527(≥) 517(≥) 42 32 21 Solution and Aging,Annealing,Ausaging,Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
683 186 472

17-4PH Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

17-4PH Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
17-4PH Coil Stock 0.08*200mm Coil or Strip Kgs 1623 Cold-Rolled+Annealed Enquiry
17-4PH Round Bar Φ5-300mm*L Round Bar Kgs 46958 Hot-Rolled+Annealed+black Enquiry