2.4856 Stainless Steels to BS EN 10095

2.4856 - Specification & Application

  • BS EN 10095 - Heat resisting steels and nickel alloys

Heat resisting steels and nickel alloys

Chemical composition(wt.%) of 2.4856 grade: to BS EN 10095

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.03 0.10
Si - 0.50
Mn - 0.50
P - 0.020
S - 0.015
Cr 20.00 23.00
Ni 58.00 -
Al - 0.30
Ti - 0.40
Fe - 5.00
Cu - 0.50
Co - 1.00
Nb+Ta 3.15 4.15

2.4856 - Detail

Heat resisting steels and nickel alloys

Mechanical properties of grade 2.4856 BS EN 10095

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
964 (≥) 295 (≥) 11 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade 2.4856 BS EN 10095

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
118 (≥) 961 (≥) 42 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
784 443 814

Equivalent Products

We can customize the production of 2.4856 grade, contact us for the best solution.