21CrMoV5-7 Stainless Steels to ISO/TR 4956

21CrMoV5-7 - Specification & Application

  • ISO/TR 4956 - Wrought steels for use at elevated temperatures in engines

Wrought steels for use at elevated temperatures in engines

Chemical composition(wt.%) of 21CrMoV5-7 grade: to ISO/TR 4956

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.25
Si - 0.04
Mn 0.40 0.80
P - 0.030
S - 0.030
Cr 1.20 1.50
Mo 0.65 0.80
Ni - 0.60
V 0.25 0.35

21CrMoV5-7 - Detail

Wrought steels for use at elevated temperatures in engines

Mechanical properties of grade 21CrMoV5-7 ISO/TR 4956

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
926 (≥) 433 (≥) 41 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade 21CrMoV5-7 ISO/TR 4956

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
378 (≥) 174 (≥) 24 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
419 454 489
We can customize the production of 21CrMoV5-7 grade, contact us for the best solution.
sales@specificsteel.com