Steels of blade for steam turbine
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.1500 | 0.2000 | ||
Mn | 0.5000 | 0.8000 | ||
P | - | 0.0200 | ||
S | - | 0.0150 | ||
Si | - | 0.5000 | ||
Ni | 0.3000 | 0.6000 | ||
Cr | 10.0000 | 12.0000 | ||
Mo | 0.6000 | 0.9000 | ||
Cu | - | 0.1000 | ||
V | 0.2000 | 0.3000 | ||
Al | - | 0.0300 | ||
N | 0.0400 | 0.0900 | ||
Nb | 0.2000 | 0.6000 |
2Cr11NiMoNbVN Steels of blade for steam turbine
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
192 (≥) | 752 (≥) | 32 | 32 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
589 (≥) | 614 (≥) | 34 | 31 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
475 | 421 | 278 |
We can customize the production of 2Cr11NiMoNbVN grade, contact us for the best solution.
–sales@specificsteel.com