2Cr20Mn9Ni2Si2N Stainless Steels to GB/T 1221 (1992)

2Cr20Mn9Ni2Si2N - Specification & Application

  • GB/T 1221 (1992) - Heat-resisting steel bars

Heat-resisting steel bars

Chemical composition(wt.%) of 2Cr20Mn9Ni2Si2N grade: to GB/T 1221 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.26
Si 1.80 2.70
Mn 8.50 11.00
P - 0.35
S - 0.03
Ni 2.00 3.00
Cr 18.00 21.00
N 0.20 0.30

2Cr20Mn9Ni2Si2N - Detail

2Cr20Mn9Ni2Si2N

Mechanical properties of grade 2Cr20Mn9Ni2Si2N GB/T 1221 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
862 (≥) 242 (≥) 21 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade 2Cr20Mn9Ni2Si2N GB/T 1221 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
735 (≥) 467 (≥) 13 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
451 246 877

Equivalent Grade

Equivalent Products

We can customize the production of 2Cr20Mn9Ni2Si2N grade, contact us for the best solution.