301S22 Stainless Steels to BS 1554

301S22 - Specification & Application

  • BS 1554 - Specification for stainless and heat-resisting steel round wire

Specification for stainless and heat-resisting steel round wire

Chemical composition(wt.%) of 301S22 grade: to BS 1554

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.00 18.00
Mo - 0.80
Ni 6.50 9.00

301S22 - Detail

Specification for stainless and heat-resisting steel round wire

Mechanical properties of grade 301S22 BS 1554

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
435 (≥) 913 (≥) 22 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade 301S22 BS 1554

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
842 (≥) 794 (≥) 33 12 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
399 631 259

Equivalent Grade

Equivalent Products

We can customize the production of 301S22 grade, contact us for the best solution.