40CAD6-10 Air 9160/C Aviation and Aero Steel to AIR 9160 C

40CAD6-10 Air 9160/C - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of 40CAD6-10 Air 9160/C grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.38 0.45
Si 0.10 0.40
Mn 0.50 0.80
P - 0.025
S - 0.020
Cr 1.50 1.80
Ni - 0.30
Mo 0.20 0.40
Al 0.80 1.30

40CAD6-10 Air 9160/C - Detail

40CAD6-10 Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade 40CAD6-10 Air 9160/C AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
921 (≥) 461 (≥) 24 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade 40CAD6-10 Air 9160/C AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
748 (≥) 286 (≥) 33 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
497 667 238

Equivalent Grade

Equivalent Products

We can customize the production of 40CAD6-10 Air 9160/C grade, contact us for the best solution.