416S 29 Stainless Steels to BS 1502

416S 29 - Specification & Application

  • BS 1502 - Specification for steels for fired and unfired pressure vessels: sections and bars
  • BS 1506 - Specification for carbon, low alloy and stainless steel bars and billets for bolting material to be used in pressure retaining applications

Specification for carbon, low alloy and stainless steel bars and billets for bolting material to be used in pressure retaining applications

Chemical composition(wt.%) of 416S 29 grade: to BS 1502

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.14 0.20
Si - 1.00
Mn - 1.50
P - 0.060
S 0.15 0.35
Cr 11.50 13.50
Mo - 0.60
Ni - 1.00

416S 29 - Detail

Specification for carbon, low alloy and stainless steel bars and billets for bolting material to be used in pressure retaining applications

Mechanical properties of grade 416S 29 BS 1502

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
832 (≥) 121 (≥) 23 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 416S 29 BS 1502

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
487 (≥) 143 (≥) 34 41 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
291 292 366

Equivalent Grade

Equivalent Products