42 2736 Special Alloy

Chemical composition%of the ladle analysis of grade42 2736

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)
0.60-0.750.20-0.500.80-1.200.0500.051.80-2.20
42 2736

Mechanical properties of grade42 2736

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
166(≥) 875(≥) 33 33 23 Solution and Aging,Annealing,Ausaging,Q+T,etc 442

Physical properties of grade 42 2736

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
779(≥) 493(≥) 13 42 11 Solution and Aging,Annealing,Ausaging,Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
266 752 321

42 2736 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

42 2736 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
SA-437 Grade B4B/SUS 616 /422 Forged Bar Dia.160xL Round Bar Kgs 2120 Forged+QT Enquiry
Stainless Steel 422 / Alloy 422 AMS 5655 UNS S42200/616/B4B Round Bar Stock Select 0 Select Enquiry